Mr Lovis in SANDBACH
Consultant Forensic Engineer & expert witness undertaking the investigation of engineering incidents & personal injury accidents for commercial, legal & insurance clients • Provision of independent & impartial expert witness evidence • Mechanical, metallurgical & non-metallic materials (i.e. polymer, composite, rubber, glass & ceramic materials) based investigations • Forensic investigations both on-site & laboratory based • Component failure analysis, including expertise in fractography & electron microscopy (SEM) • Investigat...
Miss Bagnall in MARGAM
Metallurgical failure investigation • Failure analysis of polymer and composite materials • Expertise in a range of failure mechanisms, i.e. corrosion, mechanical failure, high temperature, structural failure, welding, coatings • Particular expertise in the thermal degradation of austenitic stainless steels and nickel-based alloys • Extensive experience in corrosion mechanisms for the power, petrochemical and oil and gas industries • Forensic engineering
Dr Wright in LONDON
The forensic investigation of failed mechanical parts and machinery from general industrial/manufacturing, electrical power generation/transmission, petrochemical, automotive, water and construction industries • Collapse of cranes and large structures • Detailed experience of metal casting, reciprocating engines, gas turbines and other rotating machinery • Investigation of escapes of water/oil in domestic and commercial environments • Investigation of fractured glazing
Dr Parsons in LONDON
Investigation of engineering, materials and corrosion-related failures • Mechanical failures in load-bearing components • Glass damage • Metallurgical incidents • Analysis of fire-damaged metals • Fibre identification • Investigation of cargo damage • Cargo liquefaction cases • Incidents involving coating failures (paint) I have provided expert testimony in court in the UK, Hong Kong and Singapore.
Dr Moore in CAMBRIDGE
Weld flaws • Welding metallurgy • Welding procedures • Weld procedure qualification • Structural integrity • Engineering Critical Assessment and BS 7910 procedures • Fracture mechanics • Brittle fracture • Fracture toughness testing • Fracture and fatigue of welded structures • Steel metallurgy and microstructures
Dr Bywater in WARRINGTON
11 years of industrial experience across automotive (road vehicles and Formula 1), aluminium, refractory ceramic and defence steel heat treatment (carburising) industries • Topics are: root cause failure analysis, material selection, mechanical testing, characterisation, corrosion, molten metal corrosion of ceramics, aluminium defect and molten metal cleanliness assessment (PoDFA/Prefil), inclusion analysis, billet homogenisation assessment, manufacturing quality improvement and certification
Dr Scatigno in BRISTOL
Escapes of water, oil and gas • Building fires • Composites • Glass and ceramics • Metallurgy • Plastics/polymers • Power and energy • Geothermal
Dr Pitman in LEATHERHEAD
Materials analysis • Microanalysis using energy & wavelength dispersive X-ray analysis & interpretation of analysis results in engineering failures or materials characterisation • Scanning electron microscopy • Fractography • Hydrogen embrittlement of fasteners • Copper pipe failures • Fastener failures • Fuse failures • Metallic packaging failures (including beverage cans) • Pitting corrosion & preferential corrosion in water supply systems • Particle analysis & wear debris analysis • Electrical equipment failur...
Dr Wall in ABINGDON
Metallurgist, materials scientist, inspection and failure expert • 40 years+ experience • Experienced expert witness • Non-destructive testing and evaluation (NDT, NDE) • Failure analysis • Metallurgical analysis • Fracture mechanisms • Inspection performance & reliability • Probability of detection (POD) • Human reliability • Digitalisation • Corrosion • Cracking • Hydrogen embrittlement (HIC) • Welding defects • Steam turbine failures • Hospital pipework • Storage tanks & facili...
Dr Moody in GLASGOW
Metallurgy • Welding fabrication • Corrosion • Materials selection • Mechanical testing of materials • Identification of material damage mechanisms
Mr Hammersley in CHEADLE HULME
Consultant Forensic Mechanical & Materials Engineer & expert witness (practising since 1997, 18 years with Dr J H Burgoyne & Partners LLP (Burgoynes), 9 of which as a partner) • Forensic mechanical engineering-based investigations • Forensic metallurgical based investigations • Forensic polymer/non-metallic materials based investigations • Forensic component failure analysis, including expertise in fractography & electron microscopy • Forensic investigations into the cause of damage to equipment & machinery • Forensic ...